本文へスキップ
← Back to the glossary

知識

Don't use too much glue.

Japanese: のりはつけ過ぎない

Don't apply too much glue. It can cause bubbles or cloudiness during firing. A few dots are sufficient. Resist the urge to apply too much and use as little as possible.

Apply the fusing adhesive used to temporarily secure the layout only in small dots.

If you use too much, it can cause bubbles or cloudiness (residue) during firing.

It burns off at around 300 degrees. The glue helps it hold until that temperature is reached.

Do not apply too much glass adhesive. A few dots are sufficient.

During firing, organic matter burns, causing bubbles and cloudiness.

Since the glass pieces fuse together during firing, the adhesive is only used to hold them in place. Resist the urge to apply too much—use as little as possible.

This entry is written in Japanese by Rei Chikaoka and translated for readers outside Japan. If something reads oddly, the original is the source of truth.